Common defects in each process of cemented carbide tool manufacturing

There are still many precautions in the carbide tool manufacturing process, though cemented carbide tools are widely used in the industry. The key points of control in different process sections are also different. Only by controlling the key points of quality in each process can the production really proceed smoothly. Here are some common defects:

1. Mixing defect

During the semi-finished product stage of carbide tool manufacturing, that is, before the tool is formed, due to various reasons, the matrix powder of other brands is mixed in it. This situation is easy to confirm from the appearance after forming, and there will be obvious differences. But once this happens, it can only be scrapped.

LMM Carbide Tools, carbide tool factory, cemented carbide production, carbide tools production

2. Burr defect during carbide tool manufacturing

This defect is common in the forming stage. Because there is a gap between the mould bodies, there will be a kind of protrusion at the edge of the blade during the production process. This situation generally needs to be dealt with before sintering; otherwise, it cannot be dealt with once sintering.

3. Cracks

This is common in the press when grabbing the alloy tool during the production process. Due to excessive force, cracks are formed around the clamping hole, resulting in gaps.

4. Boat sticking (material sticking)

There are two reasons for this: one is that the mould body is left over or damaged during extrusion moulding, resulting in pits or protrusions of the same size in the same part of the extruded batch of finished products; another possibility is that the boat is sticking during the sintering moulding process.

5. Pre-sintering drop

It mainly occurs in the stage from extrusion moulding to sintering. Because of the collision, a piece will be missing at the edge of the blade. In other words, the edge of the blade is missing, which makes the shape of the product itself incomplete. Generally, this situation mainly depends on whether it will affect the use of the tool. If there is such a defect on the effective cutting edge, no matter how big or small, it is definitely unacceptable because it damages the workpiece during the cutting process.

6. Front drop

The reason why this is different from the pre-sintering drop is whether it has been sintered. In essence, the appearance of the product is incomplete and missing. It also depends on the specific location, but from the perspective of appearance recognition, if the notch is smooth and flat, it can be determined to be a front drop. If the notch is uneven, it is a pre-sintering drop. This is the difference between the two from the gap point of view. Defects in other positions depend on the defect level, that is, how big the gap is.

7. Dustfall

This usually occurs in CVD chemical coating because debris falls on the surface of the alloy tool (a bulge will be formed on the surface after the coating). The standard for judging scraping mainly depends on the size of the dust and the location of the dust.

8. Coating peeling

It is rare in CVD chemical coating, but common in PVD physical coating. It is often caused by a too-small cutting edge or target material. Of course, there are other reasons, such as excessive pressure during surface treatment of carbide tool manufacturing, and it may also be caused by unqualified surface treatment before coating. This requires specific analysis.

9. Colour difference

It occurs after the alloy tool is coated. There are many reasons for it. From its appearance, the colour of the tool body is different, making it easier to identify.

carbide tool manufacturing, Carbide rod

10. Falling after coating

This defect is very common and also occurs after the alloy tool is coated. Because the alloy tool is relatively brittle, the contact and collision between the alloy tools causes a loss at the edge of the blade. In essence, it is similar to the front fall, and there are defects in the appearance and shape.

The above are common. Of course, there are many other reasons in the production process, such as oxidation, shrinkage, corrosion, bevel grinding, single-sided grinding, uneven edge, and so on.

If you want to truly improve the quality in order to achieve the purpose of production efficiency, then these aspects need to be focused on control, especially the defects found in the coating stage after the alloy tool is formed. The defects caused at this time will directly affect the product delivery time, the pass rate and the quality of the entire line, etc.

LinkedIn
Reddit
Facebook
WhatsApp
X
Pinterest
Tumblr

Leave a Comment

Your email address will not be published. Required fields are marked *

The Main Supplier Of Cemented Carbide Products In The World

LMM Cemented Carbide specializes in the production of various types of CNC precision cutting tools such as carbide milling cutters, carbide bars, carbide drills, and carbide hobs.

Get In Touch

Contact US

The main supplier of cemented carbide products in the world