How to Reduce the Cost of Drilling? A Technical Guide

Drilling is a real cost contributor in the manufacturing industry, often accounting for 20% to 35% of the machining budget. This guide provides a practical, data-based approach that can help you reduce drilling costs by 30% to 50%. These methods have been tested in actual industry cases and are in line with relevant technical specifications, making them very reliable.

​​1. Tool Selection: Maximising Performance with Advanced Materials​​

Reduce the Cost of Drilling, metal drilling

Carbide vs. HSS Drills​​

Solid carbide drills outperform traditional high-speed steel (HSS) in nearly all applications due to:

  • ​​Superior Hardness: 1,500–2,000 HV vs. 800–900 HV for HSS.
  • ​​Higher Heat Resistance: Maintain integrity at temperatures up to 900°C (vs. 600°C for HSS).
  • ​​Extended Tool Life: 5–8x longer in hardened steels (e.g., 4140, 4340).

​​Technical Comparison​​:

Parameter Carbide Drill HSS Drill
Cutting Speed (m/min) 80–120 30–50
Feed Rate (mm/rev) 0.08–0.20 0.05–0.15
Cost per Hole* 0.15–0.30 0.50–1.20
*Based on 10,000 holes in 1045 steel.

​​Case Study​​:
A German automotive supplier machining cast iron engine blocks reduced drilling costs by 48% by switching to carbide drills. Tool life increased from 200 to 1,200 holes, lowering the cost per hole from 0.85 to 0.44.

​​2. Cutting Parameter Optimisation​​

​​Science-Backed Speed and Feed Rates​​

Optimal parameters vary by material. Below are empirically validated settings for common alloys:

Material Hardness (HRC) Speed (m/min) Feed (mm/rev) Chip Load (mm)
Mild Steel (1045) 18–22 90–110 0.15–0.20 0.18–0.25
Stainless (316L) 25–30 60–75 0.08–0.12 0.10–0.15
Titanium (Ti-6Al-4V) 32–36 40–55 0.05–0.08 0.05–0.08
Aluminium (6061-T6) 60–80 HB 150–200 0.20–0.30 0.25–0.35

​​Critical Notes​​:

  • ​​Peck Drilling: Use 0.5×D peck cycles for materials prone to work hardening (e.g., stainless steel).
  • ​​Chipbreaker Geometry: 140° split-point angles reduce thrust force by 30%, minimising tool deflection.

​​3. Coolant Strategy: Precision Over Volume​​

​​Coolant Type and Pressure​​

Effective coolant application reduces heat-induced tool wear and improves chip evacuation:

Material Coolant Type Pressure (bar) Nozzle Diameter (mm)
Steel Emulsion (5–8%) 15–20 1.0–1.5
Titanium Synthetic (MQL) 70+ 0.8–1.0
Aluminum Compressed Air N/A N/A

​​Pro Tip: For deep-hole drilling (≥10×D), use through-tool coolant with a flow rate of 10–15 L/min.

​​4. Predictive Maintenance: Avoiding Costly Failures​​

​​Tool Wear Monitoring​​
  • ​​Flank Wear (VB): Replace drills when VB reaches:
    • ​​Carbide: 0.5 mm
    • ​​HSS: 0.3 mm
  • ​​Vibration Analysis: Maintain spindle vibration below 2.5 m/s² (ISO 10816-3 standard).
​​Cost Impact​​:
  • Replacing a drill before catastrophic failure saves 500–2,000 in scrapped parts and downtime.
​​Regrinding Protocols​​
  • ​​Max Regrinds​​: 3–5 times for carbide drills (remove ≤0.1 mm per grind).
  • ​​Edge Preparation: Apply 0.02–0.03 mm T-land honing to prevent micro-chipping.

​​5. Reducing Non-Cutting Time​​

​​Quick-Change Tooling Systems​​

  • ​​Hydraulic Chucks: Reduce tool change time from 5 minutes to 30 seconds.
  • ​​Preset Tool Holders: Achieve ±0.005 mm runout with ZOLLER or Haimer presetters.

​​Case Study​​:
A Texas aerospace machine shop reduced setup time by 65% using RFID-tagged tools and automated tool changers, saving $18,000 annually.

​​6. Custom Drill Geometries for Specific Applications​​

​​Specialized Designs​​

  • ​​Oil Hole Drills​​:
    • 2–4 internal coolant channels (Ø1.0–1.5 mm).
    • Reduce heat-induced wear by 50% in 40 HRC steels.
  • ​​Step Drills​​:
    • Combine drilling and chamfering, eliminating a secondary operation.
    • Save $2.50 per part in high-volume production.

​​Coating Selection​​

Coating Thickness (µm) Best For Temp Limit (°C)
TiAlN 2–3 High-speed steel drilling 900
AlCrN 1.5–2.5 Abrasive materials 1,100
Diamond-like 0.5–1.0 Non-ferrous metals 400

​​7. Scrap Reduction through Process Control​​

​​Statistical Process Control (SPC)​​

  • Monitor hole diameter Cpk≥1.33.
  • Target tool wear within ±3σ (0.02 mm tolerance).

​​Cost Impact​​:

  • Reducing scrap rate from 5% to 1% saves $18,000/year for a shop producing 10,000 parts/month.

​​Laser Measurement Systems​​

  • Keyence LM systems inspect 100% of critical holes (e.g., aircraft engine mounts) with ±0.001 mm accuracy.

​​Case Study: Optimising Titanium Drilling

cutting tool life, metal drilling
Carbide Drill Manufacturer >>>

​​

​​Challenge​​:

  • Material: Ti-6Al-4V (HRC 36)
  • Hole specs: Ø6.35 mm × 50 mm depth, Ra ≤1.6 µm

​​Solution​​:

  • ​​Tool: Solid carbide drill with TiSiN coating
  • ​​Parameters​​:
    • Speed: 55 m/min
    • Feed: 0.06 mm/rev
    • Peck cycle: 3 mm
    • Coolant: Through-tool MQL at 80 bar

​​Results​​:

  • Tool life increased from 20 to 85 holes.
  • Cost per hole dropped from 3.20to0.75.

​​Conclusion: A Systematic Approach to Savings​​
Reducing drilling costs requires a holistic strategy:

  1. ​​Material Science: Select carbide tools matched to workpiece hardness.
  2. ​​Process Optimisation: Fine-tune speeds, feeds, and coolant delivery.
  3. ​​Preventive Maintenance: Monitor tool wear and regrind proactively.

By implementing these methods, manufacturers can achieve:

  • ​​40–60% lower drilling costs​​
  • ​​70% longer tool life​​
  • ​​Near-zero scrap rates​​

​​Final Recommendation: Conduct a drilling audit to baseline current costs (tooling, energy, scrap) and prioritise high-impact improvements.

 

LinkedIn
Reddit
Facebook
WhatsApp
X
Pinterest
Tumblr

Leave a Comment

Your email address will not be published. Required fields are marked *

The Main Supplier Of Cemented Carbide Products In The World

LMM Cemented Carbide specializes in the production of various types of CNC precision cutting tools such as carbide milling cutters, carbide bars, carbide drills, and carbide hobs.

Get In Touch

Contact US

The main supplier of cemented carbide products in the world