Due to high hardness, high brittleness and low thermal conductivity, carbide materials bring great difficulties to tool grinding, especially solid carbide cutting tools with large grinding allowances.
High hardness requires greater grinding pressure, low thermal conductivity does not allow excessive grinding heat, and high brittleness leads to a greater tendency to produce grinding cracks. Generally, when grinding carbide tools, the temperature is higher than 600℃, and the surface layer of the tool will produce oxidation discolouration, causing grinding burns of varying degrees. In severe cases, it is easy to cause cracks in the carbide tool.

Traditional silicon carbide grinding wheels for grinding carbide have been gradually phased out due to their low grinding efficiency, high grinding force, poor self-sharpening, and high local temperature on the surface of the grinding contact area, which result in poor tool edge quality, poor surface roughness, and high scrap rate.
Diamond grinding wheels are widely used in the grinding of carbide tools due to their high grinding efficiency, low grinding force, good self-sharpening, sharp diamond edges, difficulty in passivation, and low local temperature on the surface of the grinding contact area.
Analysis of the mechanism of grinding cracks in integral solid carbide cutting tools
1. Diamond grinding treatment used in the manufacture of solid carbide cutting tools can deteriorate or improve the physical-mechanical properties of the tool surface layer
The basic parameters that determine the quality of the surface layer are: micromorphology (i.e., surface roughness), structure and substructure of the surface layer, and the value and distribution of the first type of residual stress. After sintering, cemented carbide usually has a surface roughness of not less than Rz5µm. Diamond processing can ensure that Rz is not less than 2µm. In the range of Rz=1-5µm, the depth of micro-roughness does not actually affect the life index of cemented carbide.
2. The value of the first type of residual stress and its distribution along the cross section play a decisive role in the strength and life of cemented carbide
During the grinding process, the fine crystal structure parameters inside the cemented carbide grains also change, and the embedded crystal blocks are broken (coherent dispersion area), and their values are reduced by one order of magnitude. The grain micro-distortion value (Δd/d, the second type of stress) changes, and the surface layer performance also changes accordingly. However, in fact, no direct relationship has been found between the change of fine crystal structure parameters and the life of cemented carbide. Therefore, under cyclic loads (such as milling force), the service life of cemented carbide has no direct correlation with the structure and substructure of the surface layer, and is not determined by the surface roughness, but by the residual stress state of the surface layer, that is, the type I residual stress value and its distribution along the cross section play a decisive role in the strength and life of cemented carbide.
3. The shallow compressive stress distribution of the surface layer and the excessively high tensile stress value near the surface layer are the main reasons for the initiation of grinding cracks
The formation of residual compressive stress in the surface layer prompts the fracture source to migrate to the layer deeper from the surface with less load, inhibiting the initiation and expansion of cracks, which increases the strength and life; at the same time, as the depth of the residual compressive stress layer distribution in the surface layer of cemented carbide increases, its strength and life gradually increase. The residual tensile stress formed in the surface layer promotes the initiation and expansion of cracks, which is a necessary condition for the generation of cracks and reduces the strength and life.
However, the surface after grinding often has both residual compressive stress and tensile stress. Therefore, the ideal state of the grinding surface layer should be that the higher the residual compressive stress value of the surface layer, the better, and the deeper the residual compressive stress layer distribution, the better; the lower the residual tensile stress value of the near-surface layer, the better, the thinner the residual tensile stress layer, the better, and the deeper the maximum tensile stress value is from the surface, the better. On the contrary, the shallow compressive stress distribution of the surface layer and the excessively high tensile stress value of the near-surface layer are the main causes of grinding cracks.

How to prevent grinding cracks?
1) Choose an appropriate coolant and cooling method
Replace the cooling oil with a lower kinematic viscosity, improve the cooling method so that the cooling oil is always cooled in the grinding contact area, and increase the oil pump pressure of the tool grinder to enhance the cooling effect during grinding.
2) Choose the right diamond grinding wheel, a metal-bond diamond grinding wheel
Choose a medium, medium soft resin bond diamond grinding wheel or repair grinding wheel to keep the grinding wheel sharp at all times
Diamond grinding wheel concentration should be 75% to 100%, metal bond grinding wheel grit should be 120 to 140 mesh, resin bond grinding wheel (RVD) grit should be 80 to 120 mesh for coarse grinding, and 200 to 240 mesh for fine grinding.
3) Choose reasonable grinding parameters
When grinding the front and rear blades, non-feed return polishing is also used to improve the surface roughness. If imported grinding wheels are used, it is allowed to select a higher grinding wheel linear speed and a larger radial feed rate than domestic grinding wheels.
Improvement of the Grinding Process of Solid Carbide Cutting Tools
1) Reduce and avoid the generation of instantaneous high temperatures
As mentioned above, the grinding cracks on the surface of solid carbide cutting tools are mainly caused by the excessive local instantaneous temperature of the grinding contact zone during the grinding process, which forms a shallow compressive stress distribution on the grinding surface layer and an excessively high tensile stress value near the surface layer that exceeds the breaking strength of the material. Therefore, the generation of instantaneous high temperature should be reduced and avoided as much as possible during the grinding process, which also reduces and avoids the generation of residual tensile stress.
The instantaneous high temperature during the grinding process often causes changes in the mechanical properties of the grinding surface layer. This instantaneous high temperature can reach more than 1000℃, causing grinding burns on the surface layer of the tool. Grinding burns will destroy the surface layer of the tool, deteriorate the quality of the workpiece surface, and seriously affect the strength, wear resistance and service life of the tool; in severe cases, cracks will also occur.
Therefore, it is necessary not only to prevent the generation of grinding cracks but also to avoid grinding burns. During diamond processing, the local instantaneous temperature of the tool surface will depend on the processing method, diamond tool characteristics and grinding system.
2) Control and avoid grinding cracks and grinding burns
Practice has proved that the greater the linear speed and radial feed of the diamond grinding wheel, the higher the hardness of the grinding wheel, the finer the grinding wheel grain, the lower the thermal conductivity of the tool material and the more severe the grinding wheel wear, the greater the grinding temperature, and the easier it is to produce grinding cracks and grinding burns.
To control and avoid grinding cracks and grinding burns, two measures must be taken: one is to reduce the generation of grinding heat, and the other is to accelerate the transmission of grinding heat.
The way to reduce grinding heat is:
Appropriately reduce the linear speed of the diamond grinding wheel, reduce the radial feed (rough grinding-fine grinding-polishing in separate steps), select a softer diamond grinding wheel, reduce the contact area between the workpiece and the grinding wheel, reasonably select the grinding wheel grain size according to the grinding requirements, always keep the grinding wheel under sharp conditions, and select appropriate grinding coolant to reduce the friction between the abrasive particles and the workpiece.
Measures to accelerate the heat transfer

In addition to appropriately increasing the workpiece speed and axial feed rate, the measures to accelerate grinding heat transfer are mainly to adopt effective cooling methods; in order to improve the cooling effect, spray cooling, high-pressure cooling, internal cooling, and cooling oil with low kinematic viscosity can be used. In addition, during fine grinding, reducing the feed rate and appropriate polishing can effectively reduce the residual stress in the surface layer.
3) Selection of grinding parameters
In summary, in order to improve productivity and grinding efficiency, while obtaining better grinding surface quality, our method is to use a lower grinding wheel linear speed and a larger radial feed rate at the beginning, and reduce the feed rate and increase the grinding wheel linear speed for the last few times, and perform polishing, which can improve the grinding surface quality.
In order to further improve the grinding surface quality, spray cooling and high-pressure cooling can also be used, and appropriate cutting fluid can be selected. At the same time, the grinding wheel can be reasonably selected and finely dressed according to the processing object.
The principle of grinding parameter selection is:
Grinding parameters are to select a lower grinding wheel linear speed, larger radial feed, axial feed and workpiece speed as much as possible under the condition of ensuring lower grinding temperature and higher grinding surface roughness. Since the linear speed and radial feed of the grinding wheel have the greatest influence on the quality of the grinding surface layer, the steps for selecting grinding parameters are: first, select a larger workpiece speed; then select the axial feed; and finally, select the grinding wheel linear speed and radial feed.
Summary
· The main reason for the grinding cracks of solid carbide cutting tools is that the inappropriate grinding process and parameters lead to excessive local instantaneous temperature in the grinding contact area, causing excessive tensile stress values in the near-surface layer exceeding the breaking strength of the material.
· The highly sensitive hydrophilic post-emulsification fluorescent penetrant flaw detection method can effectively detect surface defects such as grinding cracks of solid carbide tools.
· The generation of grinding cracks and grinding burns can be effectively prevented by improving and optimising the grinding process and grinding parameters of solid carbide tools.