Carbide bar quality inspection can only be the measurement and verification of the physical, chemical, mechanical and mechanical properties of semi-finished products and finished products. The most important of these are the acceptance inspection of various raw materials, the testing of intermediate products and the sampling inspection of finished products, the inspection of the metallographic room, etc.
Carbide bar quality control is used to keep online products under control through the design and implementation of inspection items and process parameters for the entire manufacturing process. The focus of control is online detection and judgment, and strict implementation of the established process technology standards.
Quality management is to ensure that the raw materials, processes, equipment, personnel and environment are always under control through the design and control of the entire process from product development, and manufacturing to market service, so as to achieve continuous, stable and economic production of products that meet the design standards. The central link of management is the optimization design and optimization combination of the above five elements, and to supervise and continuously improve the implementation process.

High-quality LMM carbide bar wholesale >>
1. Physical properties and organizational structure
The main responsibility of the laboratory is online quality supervision and control, that is, quality inspection and quality judgment from the entry of raw materials into the site to the packaging of products.
The stability of cemented carbide quality depends entirely on the level of process control. The main control items are the grain size, carbon content and microstructure of the hard phase. The test items that can more sensitively reflect these control items are coercive force, cobalt magnetism and density.
The defects involved in the inspection of incense are mainly pores, graphite, η phase, mixed materials, grain abnormalities, Co pools and abnormal WC-Co structures caused by η phase.
High-quality cemented carbide bars have strict control over defects. The requirements for most products are A02B00C00E00, and the actual control level can also reach A00B00C00E00. Macro defects are generally not allowed to exist.
Therefore, by combining the four major indicators of microstructure, magnetism, cobalt magnetism and density for comprehensive analysis, the product quality can be properly evaluated and the causes of quality problems can be found.
The common quality performance problems in the production process of bars are shown in Table 1
Table 1 Common Quality Performance Problems
| Item | Deviation | Metallographic defects |
| Coercive force
HC |
High | Fine grains or decarburization |
| Low | Coarse or carburized | |
| Cobalt magnet
Com |
High | Carburization |
| Low | Decarburization | |
| Density
D |
High | η phase |
| Low | Free carbon | |
| Hardness
HV3 |
High | Fine grains |
| Low | Coarse grains | |
| Flexural strength
TRS |
Low | Carburization, decarburization, abnormal grain structure, excessive voids, poor surface processing quality or burns |
For some carbide bars with a longer outer diameter or length (extruded or isostatically pressed bars), ultrasonic testing must be used to detect whether the internal structure has macroscopic holes or cracks, provided that all physical properties meet the requirements. In addition to general structural defects, cracks are the most common and most terrible defects of bars.
2. Appearance and size of carbide bar
1) The inspection of blank size accuracy is based on the category, accuracy requirements, size characteristics, etc. of the blank, and is carried out using micrometres, vernier callipers, special inspection fixtures, etc.
(a) Carbide bar size inspection:
Length measurement: micrometre or vernier calliper (division value 0.02mm) to measure length;
Diameter measurement: use Φ6mm probe external micrometre (division value 0.01mm) to measure roundness and cylindricity;
Roundness and cylindricity measurement: use Φ6mm probe external micrometer (division value is a set of feeler gauge to measure straightness, the bar rotates on the test platform, and use a feeler gauge to measure the maximum gap between the bar and the platform)
(b) Carbide bar inspection standard:
According to the technical requirements of the drawing or the needs of the user.
2) Appearance quality standard of the blank bar (solid tool bar)
Dirty hole, gap, crack limit; (blank surface before centerless grinding) see
| Diameter ≤ 6mm | Diameter>6mm | ||
| Defect size um | Allowable number/10 | Defect size um | Allowable number/20 |
| ≥25 | 50 | ≥25 | 6.0 |
| ≥75 | 40 | ≥75 | 2.5 |
| ≥125 | 14 | ≥125 | 1.5 |
| ≥175 | 4 | ≥175 | 1.0 |
| ≥225 | o | ≥225 | 0 |
Limits of defects such as blistering, sticking (roughness), dents, etc.: max 0.10mm
For limits of defects such as edge loss: (surface of blank without centerless grinding) see
| Rod diameter (mm) | Allowable defect depth (mm) |
| D≤2.50 | 0.30 |
| D>2.50 | 0.40 |
3) Appearance inspection of centerless grinding carbide rods
The notch of PCB rods is limited to the port and the size does not exceed 0.5*0.5mm. The surface is not allowed to have defects such as unground surfaces, traces, dirt, cracks, etc.
The notch of solid tool rods is also limited to the end. The notch size of 10mm diameter is not more than 0.30.8, and the notch size of 10mm diameter is not more than 0.51.0. The surface is not allowed to have defects such as unground surface, traces, dirt, cracks, bubbles, dents, etc.
4) The size inspection standard of centerless grinding carbide rods is shown in Table 6
| Test items | Measuring tools | Testing method | Testing method | Judgment standard |
| Diameter | Micrometer, Automatic diameter measuring instrument | 20% random check
Manual/automatic |
Use a micrometre to screen according to the lower limit size and upper limit size respectively. | If no exceeding phenomenon is found, the batch of products is judged to be qualified; if 1 out of 20% exceeds the standard, double sampling is carried out; if there is still 1 exceeding the standard, an automatic monitoring instrument is used for safety inspection |
| Length | Micrometer | 20% random check
Manual |
Use a micrometer to screen twice according to the lower limit size and upper limit size respectively. | If no exceeding phenomenon is found, the batch of products is judged to be qualified; if 1 out of 20% exceeds the standard, double sampling is carried out; if there is still 1 exceeding the standard, all products in the batch are screened twice by micrometre according to the lower and upper size respectively. |
| Roundness | Roundness micrometer | 5% random check
Manual |
Use a micrometer to check the roundness of both ends of the bar | It is allowed that 2 out of 50 exceed the standard; if the requirements are not met, all the bars in the batch are reground |
| End flatness | Micrometer | 1% random check
Manual |