Titanium alloys, composed of a titanium base with added elements such as carbon, nitrogen, hydrogen, and oxygen, boast excellent physical and chemical properties, including low density, high strength, low deformation coefficient, and excellent heat and corrosion resistance. They are widely used in industries such as aerospace, aviation, shipbuilding, petroleum, chemical, automotive, and medical devices. Many countries around the world have recognized the importance of titanium alloys and have begun research, development, and application. However, these advantages also make titanium alloys difficult to machine, making many fabricators wary of them. Efficient machining of titanium alloys has become a challenging issue.
Carbide drills for titanium alloy machining are made from K40 alloy, a rod material with excellent wear resistance and impact resistance. This grade is specifically designed for machining titanium alloys, nickel-based alloys, stainless steel, and other difficult-to-machine materials. Suitable for milling and drilling, combined with a high-quality coating, they offer excellent wear resistance, long-lasting wear resistance, reduced sharpening cycles, and higher machining efficiency.
Carbide drills for machining difficult-to-machine materials like titanium alloys are suitable for high-speed machining. The drill features custom-designed curved rake, relief, and cutting edge angles, combined with a wear-resistant coating. The cutting edge undergoes a passivation treatment to eliminate micro-chipping, resulting in stronger cutting edge rigidity and a wear-resistant, chip-free drilling experience during high-speed, chip-breaking drilling. This significantly increases tool life.
Titanium alloys exhibit high strength, low deformation coefficient, high cutting temperatures, high tool tip stress, and severe work hardening. This results in tool wear and chipping during machining, making it difficult to guarantee quality.
To address the machining challenges of titanium alloys, selecting the appropriate cutting tool is crucial before designing a machining plan. Due to the material’s high strength and low deformation coefficient, the tool must possess sufficient hardness, strength, and wear resistance. Furthermore, the high cutting temperature places high demands on the tool’s thermal conductivity, and it must not exhibit chemical affinity with titanium.
Drilling is also a common process in titanium alloy machining. Burning and breakage are common problems during the drilling process. This is primarily due to poor drill sharpening, inadequate chip evacuation, poor cooling, and weak process system rigidity. Proper drill sharpening can address these issues to a certain extent.
To reduce axial forces and suppress vibration caused by drilling resistance, it is recommended to narrow the chisel edge, typically retaining a width of approximately 0.5 mm, depending on the drill diameter. The land should also be narrowed to approximately 0.5 mm 5 to 8 mm from the drill tip to facilitate chip evacuation.
The drill bit geometry must be properly sharpened, with both cutting edges maintained in perfect symmetry. The cutting edge must remain sharp at all times. If the bit becomes blunt, drilling should be stopped immediately and resharpened. Continuing to use a blunt drill bit for workpiece machining will quickly burn and anneal due to the high temperatures generated by friction, rendering the drill useless. High temperatures not only adversely affect the drill bit but also thicken the workpiece’s hardened layer, making subsequent re-drilling more difficult and requiring more drill sharpening.
Depending on the required drilling depth, the drill bit length should be minimized and the drill core thickness increased to increase rigidity and prevent chipping caused by vibration during drilling. Practice has shown that, provided the processing requirements are met, the shorter the drill bit, the longer its service life.
Drilling titanium alloys involves a semi-closed cutting process. High cutting temperatures are generated during the drilling process, resulting in significant rebound after drilling and long, thin cutting chips that tend to stick together and become difficult to remove.
For titanium alloy processing, the drill tip angle is generally increased by 135°-140°; the clearance angle at the outer edge of the drill is increased by 12°-15°; the chisel edge length is reduced by 0.08-0.1 to reduce axial forces during drilling; the helix angle p is increased by 30°-40°; and the drill core thickness is increased. Use an “S” or “X”-shaped chisel edge for drill bit sharpening, with a chisel edge length b = (0.08-0.1) do, while ensuring chisel edge symmetry ≤ 0.06 mm. Both chisel edge types create a secondary cutting edge, which acts as a chip splitter and reduces axial forces during drilling.
The external and internal cutting edge angles 2φ and 2φ’ are both 130°-140° for drill diameters do > 3-10 mm, and 125°-140° for drill diameters do > 10-30 mm. The external cutting edge clearance angle a is 12°-18° for drill diameters do > 3-10 mm, and 10°-15° for drill diameters do > 10-30 mm. The chisel edge bevel angle ψ is 45°; the internal cutting edge rake angle yr is -10°–15°; the internal cutting edge bevel angle T is 10°-15°; and the arc cutting edge clearance angle aR is 18°-20°.
Four guide lands on the drill increase the drill’s cross-sectional moment of inertia, improving rigidity and naturally forming two auxiliary cooling grooves. This increases durability by approximately three times compared to standard drills and reduces cutting temperatures by approximately 20%. Furthermore, the stable guides reduce hole expansion. For example, the hole expansion of a 3mm four-land drill is 0.03-0.04mm, compared to 0.05-0.06mm for a standard drill.