What causes uneven hardness after heat treatment of cemented carbide?

Heat treatment of cemented carbide is a very necessary process because cemented carbide has poor toughness and high brittleness, making it prone to chipping and fracture. The advent of heat treatment technology has improved the performance of cemented carbide and increased its service life. However, uneven hardness after heat treatment often occurs. Today, we will analyse the causes of uneven hardness.

Germany PVATePla, heat treatment of cemented carbide
 

1. Substandard raw material quality

For example, excessively coarse grains or decarburization on the part surface can easily lead to uneven hardness after quenching.

2. Severe structural inhomogeneities, such as unsatisfactory microstructure (such as carbide segregation or aggregation), the presence of large carbides, or large blocks of free ferrite, can directly affect surface hardness uniformity, resulting in poor hardenability and difficulty quenching thick sections, leading to uneven hardness.

3. Low quenching temperatures or short holding times, uneven furnace temperature distribution, large temperature differences within the furnace, and contact between parts that hinder heat transfer can lead to uneven heating of the parts, uneven austenite composition, insufficient carbide dissolution, incomplete dissolution of ferrite in hypoeutectoid steel, or the presence of oxide scale and salt slag on the part surface. These can also cause uneven surface hardness.

Also, prolonged heating of tungsten-containing alloy steels above 950°C can cause tungsten carbide to form within the steel, leading to uneven hardness. High-carbon and high-silicon steels can also experience graphitisation due to overheating, leading to uneven hardness.

4. Surface decarburization can occur due to the presence of a decarburized layer, oxide scale, or rust. Alternatively, the lack of vertical movement in the coolant can cause bubbles to form locally within the part, hindering the cooling process.

Carbide rod, Cemented Carbide Rod, carbide rod factory

High-quality carbide tools manufacturer >>>

5. Poor quenching: The part is not cooled quickly enough during quenching, and is not sufficiently cooled in the coolant. The cooling medium may be aged or contain impurities, such as oil, soapy water, or floating debris, which can cause bubbles to form on the part surface during cooling. Alternatively, the cooling medium may not be forced to circulate, leading to localised steam film formation and reduced cooling medium performance, resulting in uneven surface hardness after quenching.

6. Uneven Cooling of Large Parts

One possible cause is that the part does not move smoothly up and down or left and right in the cooling medium. Another possible cause is that parts accumulate during quenching, resulting in a lack of flow or agitation of the cooling medium, slowing the cooling rate and causing uneven hardness.

7. Parts quenched in water may develop uneven hardness and soft spots due to the presence of a steam film.

Testing methods include using a file, hydrochloric acid etching, and surface grinding. The appropriate method should be selected based on the specific situation. Typically, a 6- to 8-inch (1 inch = 0.0254 micrometre) medium-grain flat file is used to check hardness. For parts with a hardness above 60 HRC, the file will slip. For parts with a hardness between 58 and 60 HRC, the file will only slightly move. For parts with a hardness below 58 HRC, there will be friction between the file and the part.

 

LinkedIn
Reddit
Facebook
WhatsApp
X
Pinterest
Tumblr

Leave a Comment

Your email address will not be published. Required fields are marked *

The Main Supplier Of Cemented Carbide Products In The World

LMM Cemented Carbide specializes in the production of various types of CNC precision cutting tools such as carbide milling cutters, carbide bars, carbide drills, and carbide hobs.

Get In Touch

Contact US

The main supplier of cemented carbide products in the world